Abstract

Irreversible extrusion of Cu from through-silicon vias (TSVs) during high-temperature processing steps presents an important potential back-end-of-line (BEOL) reliability issue. Commonly this reliability risk is mitigated by introducing an anneal after Cu plating for TSV fill. This paper presents the impact of the post-plating anneal temperature and time on residual Cu pumping during a sinter for 20 min at 420 °C, for two different TSV dimensions. Using optical profilometry, in total ~ 4000 TSVs were measured, allowing detailed statistical analysis. Within one sample the Cu pumping values were found to be log normally distributed, implying an intrinsically large spread. Lower residual Cu pumping values were found in TSVs annealed at higher temperatures and for longer times, with the sinter conditions of 20 min at 420 °C confirmed as optimal post-plating anneal conditions. The larger TSVs showed more pumping in the average TSV, but at the tail of the distribution the Cu pumping behavior was the same as for the smaller TSVs. This implies that the impact of Cu pumping on BEOL reliability is identical for both sets of TSV dimensions, suggesting that the impact of Cu pumping on BEOL reliability is not necessarily reduced by reducing TSV dimensions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.