Abstract
In Ni-base superalloys with low Al and/or Ti content the precipitation and subsequent coarsening of γ′ particles at intermediate temperatures contribute to the degradation of the mechanical properties of the alloy. In the present paper the coarsening process is modelled and the change of the critical resolved shear stress of the alloy due to coarsening of the γ′ particles is calculated by means of statistical analysis of the depinning of a single gliding edge dislocation. It is found that the contribution of γ′ hardening to the critical resolved shear stress at 973 K reduces to more than half of its original value in less than one year.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.