Abstract
Orthogonal cutting of titanium alloy Ti-6Al-4V was investigated in a series of continuous and interrupted turning tests. Direct observation of the chip formation zone was achieved using a high speed imaging system with a long-distance microscope lens. Frame rates from 20,000 to 50,000 frames per second were used to record the chip formation cycle over a range cutting speeds from 4 to 150 m/min and at feeds of 0.05, 0.075 and 0.1 mm. Strobed laser illumination was used to avoid image blurring. Visual images of the chip formation cycle were synchronised with recording of the cutting and feed forces. Segmented chips were observed throughout the investigation and image analysis of the recorded video sequences allowed the determination of the chip velocity, the shear angle, the segmentation frequency, the critical strain for shear band initiation and the shear strain within the shear bands.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.