Abstract

Copper foil impurities are hampering scalable production of high-quality graphene by chemical vapor deposition (CVD). Here, we conduct a thorough study on the origin of these unavoidable contaminations at the surface of copper after the CVD process. We identify two distinct origins for the impurities. The first type is intrinsic impurities, originating from the manufacturing process of the copper foils, already present at the surface before any high-temperature treatment, or buried into the bulk of copper foils. The buried impurities diffuse towards the copper surface during high-temperature treatment and precipitate. The second source is external: silica contamination arising from the quartz tube that also precipitate on copper. The problem of the extrinsic silica contamination is readily solved upon using an adequate confinement the copper foil samples. The intrinsic impurities are much more difficult to remove since they appear spread in the whole foil. Nevertheless, electropolishing proves particularly efficient in drastically reducing the issue.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.