Abstract

Cation vacancies on both sublattices (V(Ti), V(Sr)) have been identified in homoepitaxial pulsed laser deposited SrTiO3 films using high intensity variable energy positron annihilation lifetime spectroscopy (PALS) measurements. Film nonstoichiometry was varied by varying laser fluence. PALS showed that on increasing the fluence above the Ti/Sr∼1 value, the concentration ratio [V(Sr)]/[V(Ti)] systematically increased. Reducing the fluence into the Ti-poor region below resulted in additional vacancy cluster defect formation. Vacancy concentrations greater than ∼50 ppm were observed in all films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.