Abstract

A method was developed for combined treatment of a hydroxyapatite gel in its secondary maturation stage by reacting the gel with a dilute phosphoric acid solution to pH 7.6 and subsequently with distilled water to pH 7.0–7.2. The method allows decreasing 1.2–1.7-fold the time of the secondary maturation of hydroxyapatite gel, and 2.5-fold, the amount of the washing solution, whereby a single-phase hydroxyapatite or a hydroxyapatite containing up to 11% of α-tricalcium phosphate can be prepared.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.