Thirty millimeter ZnO single crystals have been grown by the hydrothermal method with new mineralizers and a low-cost liner. A sharp X-ray rocking curve with the full width at half-maximum of 36 arcsec has been obtained for the (002) reflection, indicating a good crystallinity of the crystal. Low temperature photoluminescence spectrum revealed the crystal has a narrow and strong free exciton emission band (3.359 eV) at 10 K, with the absence of a green-yellow emission band that generally is induced by the impurities or lattice vacancies. Compared to ZnO crystals hydrothermally grown from conventional mineralizers (LiOH and KOH), this crystal has a unique feature that the room-temperature carrier mobility is close to the intrinsic value, with the carrier concentration maintained as high as 4.09 × 1016 cm−3. Two main donors which may relate to the H impurity were indicated. Analysis revealed that the diffusion of H in the ZnO lattice might be responsible for the decrease in conductivity of the ZnO crystal after annealing. The reason why the new hydrothermal method yielded low-resistance ZnO crystals could be interpreted as a much higher concentration of H impurity and much lower concentration of Li impurity incorporated into the ZnO lattice, compared with samples yielded by the conventional hydrothermal method. We anticipate the reported high-quality ZnO single crystals can not only be suitable objects for studying the intrinsic properties of ZnO, but also be potential substrates for fabricating ZnO light emitting diodes devices.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call