AbstractReactive silica materials like vitreous silica or cristobalite were dissolved at temperatures between 100 and 220 °C for up to 7 days in NaOH lyes. The liquid and solid reaction products were analyzed chemically. Sodium water glasses with silica concentrations of up to 27 wt % and molar SiO2/Na2O ratios of up to 3.7 were obtained. The experimental data were evaluated by an approximation algorithm. The initial size reduction rates ranged between 0.1 and 7 µm h−1, depending on the temperature and the choice of starting materials. Correlations between thermodynamics and kinetics were discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.