Abstract

Poly(ester-co-amides), PBSe random copolymers, were prepared by polycondensation of sebacic acid and 1,4-butanediol, introducing 1,4-butanediamine as comonomer. The homopolymer was semi-crystalline with T m of 65 °C. When the amide content was over 10%, two melting endotherms were observed and their melting enthalpies decreased significantly. WAXD results also showed a decrease of crystallinity with increasing amide content. Poly(ester-co-amides) had intramolecular and intermolecular hydrogen bonding, which was conformed by FT-IR. The degradability of the PBSe series increased with the amide content. Quantitative FT-IR analysis shows that the areas of the amide-amide hydrogen bonded NH band increased but the areas of amide-ester hydrogen bonded NH band decreased during hydrolysis.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.