A systematic study on the degradation and drug release from L-lactic acid and ricinoleic-acid-based copolyesters is reported. These copolyesters were synthesized by ring opening polymerization (ROP), melt condensation (COND) and transesterification (TRANS) of high molecular weight poly(lactic acid) (PLA) with ricinoleic acid (PLA-RA), and repolymerization by condensation to yield random and block copolymers of weight average molecular weights (Mw) between 3000 and 13,000. All polymers showed an almost zero-order weight loss, with a 20-40% loss after 60 days of incubation. Lactic acid release to the degradation solution is proportional to weight loss of the polymer samples. The main decrease in molecular weight was observed during the first 20 days, followed by a slow degradation phase, which kept the number average molecular weight (Mn) at 4000-2000 for another 40 days. Water-soluble 5FU was released from ricinoleic-acid-based polymers faster than slightly water-soluble triamcinolone. Drug release into phosphate-buffered saline (pH 7.4, 0.1 M) at 37 degrees C from P(LA-RA) 60:40 prepared by condensation of the acids was faster than from pasty P(PLA-RA) 60:40 synthesized by transesterification for both drugs.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.