In the present work positron lifetime spectroscopy was employed for investigation of hydrogen-induced defects in Pd. Well annealed polycrystalline Pd samples were electrochemically charged with hydrogen and the development of defects with increasing hydrogen concentration was investigated. At low concentrations (α-phase region, xH<0.017H/Pd) hydrogen loading introduced vacancies surrounded by hydrogen atoms and characterized by a positron lifetime of ≈200ps. When the hydrogen concentration exceeded 0.017H/Pd the α-phase transformed into the hydrogen rich α′-phase. This generated dislocations characterized by a positron lifetime of ≈170ps. Dislocations can accommodate a large volume mismatch between the α and the α′-phase. Hardness testing revealed that absorbed hydrogen made Pd harder. In the α-phase region hardness increased due to solid solution hardening caused by dissolved hydrogen. Dislocations created by the α to α′-phase transition caused strain hardening which led to an additional increase of hardness.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.