ABSTRACTWe successfully grow high-quality hydrogenated amorphous-silicon-germanium alloys (a-SiGe:H) by the hot-wire chemical-vapor deposition (HWCVD) technique using silane and germane gas mixtures. These alloys display electronic properties as good as those grown by the plasma-enhanced chemical-vapor deposition (PECVD) technique, when comparing materials with the same optical bandgaps. However, we grow materials with good electrical properties at high deposition rates—up to 40 Å/s, compared to 1–4 Å/s for PECVD materials. Our alloys exhibit similar trends with increasing Ge content to alloys grown by PECVD. The defect density, the dark conductivity, and the degree of nanostructural heterogeneity (as measured by small-angle X-ray scattering) all increase with increasing germanium content in the alloy. The nanostructural heterogeneity displays a sharp transition between 9 at.% and 14 at.% germanium. PECVD- grown a-SiGe:H alloys exhibit a similar transition at 20 at.% Ge. The photoconductivity and the ambipolar diffusion length of the alloys decrease with increasing germanium content. For a fixed silane-to-germane gas ratio, all material properties improve substantially when increasing substrate temperature (Tsub) from 220°C to 375°C. Increasing Tsub also narrows the optical bandgap and lowers the hydrogen content in the alloys for the same germane-to-silane gas ratio.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.