Abstract

With the aid of hydrogen permeating devices, the hydrogen permeation behaviors of X52 pipeline steel in NACE A solution with saturated H2S/CO2 were studied under the conditions of different ambient temperatures and pH values, and the hydrogen permeation behaviors of X52 pipeline steel in weld seam zone were comparatively studied. The experimental results show that the hydrogen permeation coefficient value is directly proportional to the time required for reaching the saturation anode current and inversely proportional to the saturation anode current, and the hydrogen permeation coefficient is influenced by the corrosion scales; the temperature is directly proportional to the saturation anode current, and the hydrogen permeation coefficient is influenced by the temperature and corrosion scales, heat-affected zone and matrix zone in NACE A solution with saturated H2S/CO2 at normal temperature. The hydrogen permeation coefficient in weld seam zone is larger than that in heat-affected zone which is further larger than that in matrix zone.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.