Abstract
We show strong changes in chemical etching of phosphorus-doped fiber cores due to hydrogen loading and subsequent UV-irradiation using an atomic force microscope. The etch rate of the fiber core in a low concentration hydrofluoric acid solution (HF) is decreasing after hydrogen loading by as much as 30%. In contrast, UV-irradiation of the hydrogenated fiber increases the core etch rate to values of 27% above the etch rate of the pristine fiber. The UV-induced change in etch rate does not depend on pulse fluence, but only on total dose. We attribute the changes in etch rate to a hydrogen- and radiation-induced modification of color center population.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.