Chemical stability of multiferroic BiFeO 3 (BFO) ceramics has been studied through electrochemical hydrogen charging, in which BFO ceramic pellets were placed in 0.01 M NaOH solution with hydrogen deposited on their electrodes from the electrolysis of water. The properties of the samples were greatly degraded after the treatment: The leakage current was increased by orders of magnitude, the capacitance and the dielectric loss were dramatically increased in low frequency region. It was proposed that hydrogen entered into BFO lattice and existed at interstitial sites and the degradation was explained by hydrogen's reduction of some Fe 3+ to Fe 2+ in BFO. Hydrogen-induced degradation occurs relatively easily in BFO and much attention should be paid to it for BFO-based devices.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.