Abstract

The hydrogen-induced-cracking (HIC) behaviour of the magnesium alloy AZ80 was evaluated using the slow strain rate test method. The study shows no evidence of HIC in AZ80 alloy after pre-exposure or pre-charging in distilled water. However, under continuous charging in distilled water during straining, the AZ80 alloy shows evidence of HIC. The contradiction reported in the literature is addressed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.