Abstract
Hydrogen Induced Cracking and Sulphide Stress Corrosion Resistance of High Strength Line Pipe Steels for Sour Gas Application
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
https://doi.org/10.2174/2352094906666160922143127
Publication Date: May 2, 2017 |
Hydrogen Induced Cracking and Sulphide Stress Corrosion Resistance of High Strength Line Pipe Steels for Sour Gas Application
Join us for a 30 min session where you can share your feedback and ask us any queries you have