Hydrogen embrittlement (HE) behavior was investigated in a low carbon medium Mn steel with three different volume fraction of retained austenite (RA), which was obtained after different heat treatments. The hydrogen permeation test showed a higher permeability for directly water quenched specimen compared to quench-tempered specimens. Melt extraction test showed hydrogen concentration increased with hydrogen charging current density in the order of directly quenched specimen, QLA, quenched with low-temperature annealed specimens and QHA quenched with high-temperature annealed specimens. Slow strain-rate tensile test was employed to examine the HE behavior, the HE indices decreased with the increase of RA irrespective of increased hydrogen concentration. HE susceptibility can be suppressed by raising intercritical annealing temperature because Mn enrichment increases the stability of RA.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.