Abstract

The effects of deformation on the hydrogen absorption/desorption behavior of a B2 single-phase Ti–22Al–27Nb (at.%) alloy were investigated mainly by measuring the static pressure–composition ( P– C) isotherms from room temperature to 100°C for specimens quenched from 1200°C and deformed to 5–∼90% in compression or by cold-rolling. β hydride is formed at a very low hydrogen pressure similarly to bcc hydrogen absorbing alloys. In as-quenched specimens, further absorption to γ hydride is sluggish and there is no obviously reverse γ→β hydride transformation. Both the β→γ and reverse γ→β hydride transformations are promoted by deformation. The best hydrogen absorption/desorption properties are attained in specimens deformed to 5–10%, the deformation structure of which consists of well-aligned and uniformly distributed <111> screw dislocations. The beneficial effects of deformation on the hydrogen absorption/desorption behavior of the alloy are interpreted in terms of similarities between atomic displacements around straight screw dislocations and those taking place during the β–γ hydride transformation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.