Hydrogen and hydrazine co-injection into a boiling water reactor was considered as a new mitigation method of stress corrosion cracking. To confirm decrease of electrochemical corrosion potential by the reduction of oxygen and hydrogen peroxide in bulk water using reducing agent, reaction of hydrazine with oxygen or hydrogen peroxide under simulated downcomer conditions (temperature: 280°C, duration: 4.2 s and gamma-irradiation) was examined. All the oxygen was consumed above the equivalent concentration for the reaction with oxygen within this short time (gamma-irradiation case) and almost all the hydrogen peroxide was consumed. Reaction rates were accelerated more than five times by gamma-irradiation in each case. Reaction rates with oxygen were compared with other reducing agents such as hydrogen, methanol and ammonia. From the viewpoint of reaction rate and formation of by-product, hydrazine was the most suitable agent. Using a simple model based on the experimental results, water chemistry for the bottom region was calculated for the case of no hydrogen injection and for the case of 0.2 mmol-kg−1 hydrogen injection into feed water. For both cases, concentrations of dissolved oxygen and hydrogen peroxide were estimated to decrease enough to mitigate SCC, with concentration of ammonia suppressed below the management criteria for reactor water chemistry.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.