Abstract
Two series of unsymmetrical hybrid benzoxazines were separately synthesized using combinations of natural bio-phenolic materials, namely cardanol (C) with eugenol (E), vanillin (V), and guaiacol (G) using diaminodiphenylmethane (ddm)/diaminodiphenyl ether (dde) through the well-known Mannich reaction. The synthesized hybrid benzoxazines have a cure temperature between 229 °C and 269 °C. Compared to previous synthesized benzoxazines, vanillin-based benzoxazines (C-dde-V and C-ddm-V) have a lower cure temperature. TGA results show that poly(C-ddm-V) and poly(C-dde-V), two hybrid polybenzoxazines, have superior thermal stability than the other hybrid polybenzoxazines. In order to develop polybenzoxazine composites, different wt% of GPTMS functionalized vermiculite was incorporated with poly(C-ddm-V). The properties of these composites were examined and contrasted with those of a neat matrix. The hybrid polybenzoxazines and composites water contact angle values vary from 136° to 144°, suggesting that all of the hybrid polybenzoxazines and composites have good hydrophobic behavior. On increasing the concentration of vermiculite, the dielectric constant value significantly decreased to a low dielectric constant.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Journal of Polymer Analysis and Characterization
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.