Abstract

This study investigated the leaching of monomers (Bis-GMA and TEGDMA) from nano-hybrid (Filtek Supreme) and flowable (Filtek Flow) dental composite resins cured with LED or conventional halogen curing lights, and immersed in saliva or water for 24 h. Nine disc specimens were made for each experimental group. After the polymerization process, the specimens were immersed in either water or saliva and incubated at 37 degrees C for 24 h. Eluted Bis-GMA and TEGDMA monomers were detected using high performance liquid chromatography (HPLC). The data were analyzed using three-way ANOVA (p = 0.05) and the independent samples t test. TEGDMA (53.15-1 microg/L) was leached from the resins at a higher level than Bis-GMA (28-0.5 microg/L) (p < 0.01), regardless of the affecting factors: composite type, solvent (media) and type of curing light. In general, Filtek Flow resin released more TEGDMA than Filtek Supreme (p < 0.05), but the Supreme resin released more Bis-GMA than TEGDMA (p < 0.05). Halogen light induced greater monomer elution than LED light immersion in water. Saliva released more TEGDMA than water (p < 0.05). We conclude that (1) total leached TEGDMA was higher than total Bis-GMA, (2) saliva and halogen light (lower intensity than LED) leached more monomers from the resins, and (3) the flowable composite resin leached more TEGDMA than the nano-hybrid.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.