Abstract

Large green single crystal diamond with high nitrogen concentration is firstly synthesized by temperature gradient method under high pressure and high temperature (HPHT). Sodium azide (NaN 3) is added as the source of nitrogen to the synthesis system of high pure graphite and kovar alloy (Fe 59Co 25Ni 17). The HPHT synthesis condition is 5.4 GPa and 1480 K. The maximum crystal size is 3.2 mm. The infrared absorption spectra indicate that the nitrogen concentration in the green large single crystal diamond reaches 1520 ppm in the form of single substitution, which is close to that in nature diamond, and several times higher than that in the man-made Ib large single crystal diamond previously.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.