Abstract

The G3 and 825 alloys, with excellent combination of mechanical properties and corrosion resistance, can be used in hot, and acid environments. Thermal simulation tests were conducted on the alloys G3 and 825 in the THERMECMASTOR-Z simulator, at temperature between 1030 and 1300 °C, with strain rate from 1 to 50 s −1 and strain ɛ=0.8. The variations of flow stress with deformation temperature and strain rate were presented. Change of alloy structure with hot deformation and effect of strain rate on alloy dynamic recrystallization have been studied through microstructure observation by OM, SEM and TEM. Moreover, hot plasticity characteristics of alloy were analyzed by temperature-reduction of area curves. The results showed that available hot working temperature for G3, G3-Z and 825 was 1 100 to 1 240 °C, 1 130 to 1 220 °C and 1 050 to 1 240 °C, respectively. The reliable information on hot working in the alloy pilot production in steelwork is given.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.