Abstract

The hot stamping of α+β titanium alloy sheet into U shape with concave bottom using resistance heating were performed. Since both edges of the sheet in contact with a pair of electrodes were not heated, cracks occurred around the corners of the bottom due to the partially high flow stress. The cracks were prevented by slitting both edges before resistance heating because of the elongation of the edges. In addition, the hot stamping of titanium alloy sheet into joggle using partial resistance heating were performed. The distortion of sheet was reduced by reduction in area of resistance heating

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.