Abstract
The construction of inorganic nanostructures with hollow interiors is demonstrated by coating self-assembled polymeric nano-objects with a thin Al2O3 layer by atomic layer deposition (ALD), followed by removal of the polymer template upon heating. The morphology of the nano-object (i.e., spherical or cylindrical) is controlled by the block lengths of the copolymer. The thickness of the Al2O3 wall is controlled by the number of ALD cycles.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.