Abstract
We investigated the Hirschfeld surface analysis and critical behaviour in La0.5Ca0.4Ag0.1MnO3 near the second-order ferromagnetic phase transition at Curie temperature TC. We determined the critical exponents, β, γ and δ corresponding to the temperature dependence of spontaneous magnetization, initial susceptibility and isothermal magnetization, respectively. The study of Hirshfeld surface reflects that both the electrostatic and intermolecular interactions are short range. The values for critical exponents obtained from magnetic measurements are very close to those predicted by the mean field tri-critical model. The critical-exponent values deduced here were in a good conform to those obtained using the modified Arrott plot and Widom scaling relation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.