Abstract

Nano-copper sintering is one of new die-attachment and interconnection solutions to realize the wide bandgap semiconductor power electronics packaging with benefits on high temperature, low inductance, low thermal resistance and low cost. Aiming to assess the high-temperature reliability of sintered nano-copper die-attachment and interconnection, this study characterized the mechanical properties of sintered nano-copper particles using the high-temperature nanoindentation tests. The results showed that: firstly, the hardness and indentation modulus of the sintered nano-copper particles increased rapidly when the loading rate increased below 0.2 mN·s−1 and then stabilized, and decreased with increased applied load up to 30 mN. Next, by extracting the yield stress and strain hardening index, a plastic stress–strain constitutive model at room temperature for sintered nano-copper particles was obtained. Finally, the high temperature nanoindentation tests were performed at 140 ˚C–200 ˚C on the sintered nano-copper particles prepared under different assisted pressures, which showed that a high assisted pressure resulted in the reduced temperature sensitivity of hardness and indentation modulus. The creep tests indicated that high operation temperature resulted in a high steady-state creep rate, which negatively impacted the creep resistance of sintered nano-copper particles, while the higher assisted pressure could improve the creep resistance.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.