High-temperature (1550°C) creep tests are performed on tubular thin-walled specimens of single-crystal molybdenum loaded by internal pressure in a 1849P-1/2500 unit with a number of modifications. Strains are measured periodically in the circumferential and axial directions. Test results are processed statistically by two methods.