Abstract

Sixteen wide-plate crack-arrest tests have been completed, ten utilizing specimens fabricated from A533B Class 1 material and six fabricated from a low-upper-shelf base material. Each test utilized a single-edge notched specimen that was subjected to a linear thermal gradient along the plane of crack propagation. Test results exhibit an increase in crack-arrest toughness ( K Ia ) with temperature, with the rate of increase becoming greater as the temperature increases. When the wide-plate test results are compared with other large-specimen results, the data show a consistent trend in which the K Ia data extend above the limit provided in ASME Section XI.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.