Abstract

ABSTRACT The work presents the results of high-temperature brazing of reduced activated ferritic martensitic steel EK-181 with pure tungsten, which is essential for DEMO fusion reactor. To reduce thermal stresses, vanadium interlayer was used. Brazing alloys to be used were rapidly quenched into ribbons Cu-28Ti and Cu-28Sn for EK-181/V, Cu-50Ti for V/W. Microstructure investigations, mechanical and thermocycling test were carried out. It is shown that Cu-28Ti is better to use; however, it is necessary to improve the reliability of V/W seam.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.