Slot waveguide based ring resonators filled with atomic layer deposited (ALD) aluminum oxide (Al2O3) were fabricated and characterized. Our results demonstrate that ALD can be used to create slot waveguide ring resonators with relatively high Q-factors, which opens new possibilities for various photonic applications, such as optical sensing and all-optical signal processing.