Abstract
Nanoporous iridium electrodes are prepared and electrochemically investigated towards the water oxidation (oxygen evolution) reaction. The preparation is based on ‘anodic’ aluminum oxide templates, which provide straight, cylindrical nanopores. Their walls are coated using atomic layer deposition (ALD) with a newly developed reaction which results in a metallic iridium layer. The ALD film growth is quantified by spectroscopic ellipsometry and X‐ray reflectometry. The morphology and composition of the electrodes are characterized by scanning electron microscopy, energy‐dispersive X‐ray spectroscopy, and X‐ray diffraction. Their catalytic activity is quantified for various pore geometries by cyclic voltammetry, steady‐state electrolysis, and electrochemical impedance spectroscopy. With an optimal pore length of L≈17–20 μm, we achieve current densities of J=0.28 mA cm−2 at pH 5 and J=2.4 mA cm−2 at pH 1. This platform is particularly competitive for achieving moderate current densities at very low overpotentials, that is, for a high degree of reversibility in energy storage.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.