Abstract

The direct F2-gas fluorination of mesoporous silica is a unique method leading to high fluorinated (up to 13 wt % F) and homogeneous powder with a controlled amount of grafted fluorine. Thermogravimetric analysis coupled with mass spectrometry for water, hydroxyl, and fluorine groups have allowed concluding that low fluorine-grafted silicas are thermically stable up to 550 °C whereas high fluorine-grafted silicas start to decompose from 250 °C with departure of SiF4 species. Water adsorption measurements have demonstrated the hydrophobic character of fluorinated silica and proved that direct fluorination is a way to control the hydrophilic−hydrophobic balance of silica. Pristine and fluorinated silicas have been studied by 19F and 1H MAS, and 1H−29Si and 19F−29Si CP-MAS NMR spectroscopies. NMR measurements have revealed various tetrahedral (O2/2SiF2, O3/2SiF) and pentahedral (O4/2SiF) fluorosilicate species previously observed in moderately fluorinated silica, and two unprecedented pentahedral species occ...

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.