The waste sulfuric acid solution generated from titanium dioxide production is called titanium dioxide waste acid (TWWA), which is an important resource for scandium production. A way including enrichment and purification stages for recovery and purification of Sc from TWWA with 10% P204 - 5% TBP synergistic extraction system was studied. In the enrichment stage, the preferred experimental conditions were obtained, i.e., the A/O ratio: 30, 25 °C, contact time: 30 min. In the following purification stage, the above-obtained enrichment products by stripping with 5 M NaOH were dissolved with 3 M HCl with 1% H2O2 added. The added H2O2 can lead to Ti form peroxy complex ([TiO(H2O2)]2+) that can effectively inhibit its co-extraction into the oil phase. The optimized purification conditions were the A/O ratio of 5, 30 min and 11 mmol/L Sc concentration. The stripping products obtained from the purification stage were dissolved with 2 M HCl, and then 0.5 M H2C2O4 was added to precipitate scandium. After washing and calcining, a product of 99.28% Sc2O3 was obtained. The recovery rate of scandium in the whole process was 90.34%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.