The possibility of using direct pumping into the emitting level of the Nd3+ ion in magnesium-compensated strontium lanthanum aluminate (Sr(1-x)La(x-y)Nd(y)Mg(x)Al(12-x)O19) to improve 900 nm 4F(3/2) --> 4I(9/2) laser emission is discussed. Selection of the composition parameters x and y for optimization of laser emission and reduction of heat generation is based on the spectroscopic and crystal growth characteristics. Pumping in the 865.5 nm absorption band 4I(9/2)(Z1) --> 4F(3/2)(R1) transforms the laser process into a quasi-two-level scheme of very low (below 4%) quantum defects. A very high slope efficiency (over 84%) for 901 nm continuous-wave laser emission is demonstrated with Ti:sapphire laser pumping in this band for a crystal with x = 0.4 and y = 0.05.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.