Sub-10 nm technology node manufacturing processes may require the use of thicker and denser TiN hard mask for patterning at the BEOL. The modified TiN, which tends to be more chemically robust, must be removed using a wet etch process, while maintaining typical throughput - no extension of typical wet etch process times. To satisfy these needs, a new TiN etching accelerator was found that enhanced the activity of peroxide-related species in a wet etch chemical formulation that achieved increased TiN etch rate relative to formulation without TiN etch rate accelerator (Sample 1), while also minimizing the damage to ultra-low-k inter layer dielectric (ILD) layer by a strong base, also present in the formulation. We report here the result of a solvent based formulation, which adopted the TiN etching accelerator. The formulation was able to maintain TiN etch rate and remove post-etch residue, while remaining selective to ultra-low-k ILD, Co and Cu. The TiN etch rate of the accelerator enhanced formulation can be further tuned by modifying the process temperature or the hydrogen peroxide to formulation mixing ratio and has the potential capability to process > 400 wafers.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.