Plasma surface alloying (PSA) technique was employed with nickel as incident ions to prepare the TiNi/Ti2Ni alloyed layer on surface of Ti6Al4V. High-temperature friction and wear performance of TiNi/Ti2Ni alloyed layer and the Ti6Al4V substrate were evaluated at 500[Formula: see text]C. The results indicated that the TiNi/Ti2Ni alloyed layer exhibited superior high-temperature wear performance. The variations of friction coefficient were the same rule but wear rate was lower compared to Ti6Al4V substrate. The wear mechanism of TiNi/Ti2Ni alloyed layer was mainly slight abrasion and the Ti6Al4V substrate showed abrasion and oxidation wear. The friction coefficient of the TiNi/Ti2Ni alloyed layer decreased from 0.90 to 0.50 with the increase of temperature from room temperature to 500[Formula: see text]C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.