Magnetic hysteresis of YBa/sub 2/Cu/sub 3/O/sub 7-/spl delta// thin-film pickup loops was measured using a single-layer sample design that allowed experiments to characterize both magnetometers and gradiometers. Measurements were performed at 77 K for samples having pickup-loop linewidths ranging from 20 /spl mu/m to 800 /spl mu/m. Magnetometer hysteresis was found to increase with increasing linewidth and increasing amplitude of the applied magnetic field ramp. Gradiometer hysteresis was found to depend primarily on the degree of hysteretic balance between the two individual loops comprising the gradiometer. The dependence of gradiometer hysteresis on applied field amplitude was found to be sample dependent, monotonically increasing in some cases, and exhibiting a local minimum in others.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.