Abstract

High temperature reduction generally induces the sintering of supported noble metals, therefore resulting in a negative effect on their performance. Here, we show that high temperature reduction was able to dramatically increase the activity of Pd/TiO2 for ambient HCHO oxidation. We prepared a Pd/TiO2 catalyst and pre-reduced it with H2 at low temperature (300°C) and high temperature (450°C), respectively, and then tested the activity for HCHO oxidation at ambient temperature. The Pd/TiO2-450R catalyst showed a much better performance than Pd/TiO2-300R at room temperature. 100% HCHO conversion could be obtained on the Pd/TiO2-450R catalyst at a GHSV of 95000h−1 and 140ppm inlet HCHO. The catalysts were then characterized by using Brunauer-Emmett-Teller (BET), X-ray diffraction (XRD), High-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) and other methods. The results indicate that high temperature reduction could induce the strong metal-support interaction (SMSI), decreasing the surface Pd particle size by partially encapsulating and trapping Pd clusters with TiO2, and also could produce more oxygen vacancies, beneficial to the activation of O2 and formation of surface OH groups, opening a more effective pathway for ambient HCHO oxidation. Therefore, the Pd/TiO2-450R catalyst demonstrated high activity for ambient HCHO oxidation.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call