Abstract

The internal friction of a cold-rolled Fe-Mn-Si alloy has been investigated using a multifunctional internal friction apparatus though forced vibration method from room temperature to 950 °C. It has been shown that an internal friction peak is found on the IF-T curves during first heating at around 640 °C for the cold-rolled Fe-Mn-Si alloy. The internal friction peak is confirmed to be crystallizing peak of amorphous. The amorphous is resulted from the cold-rolling of the Fe-Mn-Si alloy.

Full Text
Published version (Free)