This study investigates the effect of microstructure on short-term and long-term oxidation behaviours of GH3536 superalloy fabricated by laser powder bed fusion (LPBF), in which the superalloy is isothermally oxidised at 950 °C for 6 h and 500 h in air. The LPBF sample exhibits improved oxidation resistance compared with a wrought counterpart after long-term exposure. The effect of microstructure diversity between LPBF and wrought samples on oxidation behaviour is discussed. The cellular structure produced during the LPBF process acts as a rapid diffusion path to accelerate the formation of a protective film in the initial stage, leading to an enhancement in oxidation resistance for extended exposure.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.