We use in-situ heated nanoindentation to investigate the high-temperature nanomechanical properties of epitaxial and textured ZrB2 films deposited by magnetron sputtering. Epitaxial films deposited on 4H-SiC(0001) show a hardness decrease from 47GPa at room temperature to 33GPa at 600°C, while the reduced elastic modulus does not change significantly. High resolution electron microscopy (HRTEM) with selected area electron diffraction of the indented area in a 0001-textured film reveals a retained continuous ZrB2 film and no sign of crystalline phase transformation, despite massive deformation of the Si substrate. HRTEM analysis supports the high elastic recovery of 96% in the films.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.