Abstract

We synthesized lead-free ([Formula: see text]CaZrO3–[Formula: see text]SrTiO3 solid-solution ceramics and studied their structure, dielectric and energy storage properties. X-ray diffraction and scanning electron microscope reveal the microstructure of the samples. A high temperature dielectric relaxation behavior at the temperature ranges of 200[Formula: see text]C–550[Formula: see text]C is found for [Formula: see text], 0.5 and 0.7 samples. We explore that the origin of high temperature dielectric relaxation behavior is related to the migration of oxygen vacancies by Arrhenius law and oxygen treatment experiment. Moreover, with the increase of SrTiO3 content, the 0.3CaZrO3–0.7SrTiO3 exhibits high dielectric constant ([Formula: see text] at 1 kHz), low dielectric loss ([Formula: see text] at 1 kHz), good energy density ([Formula: see text] J/cm[Formula: see text] and high efficiency ([Formula: see text]%) simultaneously, and the possible causes of energy storage behavior dependence are analyzed in detail.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.