Abstract

The four-point bending creep properties of a hot-pressed β-sialon with Sm–melilite solid solution (denoted as M′) as intergranular phase have been studied in the temperature range 1250–1350°C in air. Creep rates plotted against stresses gave stress exponents of 1.45, 1.51 and 1.72 at 1250, 1300 and 1350°C, respectively, and Arrhenius plot between creep rate and temperature yielded a creep activation energy of 576 kJ mol −1. Cavities were found to be mainly on the triple grain junctions. Diffusion coupled with grain boundary sliding and accompanied by the formation of wedge-shaped cavities was identified as the dominant creep mechanism.