Nano-multilayered TiAlSiN films with a composition of 26Ti-16.3Al-1.2Si-56.5N (at.%) were deposited onto steel via arc ion plating, and corroded at 800-900 °C for 30 h in Ar-0.2%SO2 gases. The films were corrosion resistant, because the oxidation process dominated sulfidation. The scales consisted primarily of Al2O3 and TiO2, where a small amount of Si dissolved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.