Abstract

Axial insulation breaks are needed in ITER superconducting magnet system, which are used for separation of high voltage area from grounded cooling pipes system. To determine the maximum safe temperature that the insulating break can withstand without damage, such as preventing damage by overheating during welding of the insulating breaks to the helium cooling pipes for the superconducting magnets and high temperature baking to remove moisture, the glass transition temperature was tested by using the dynamic mechanical analysis with the standard sample made from epoxy resin. Furthermore, the high temperature baking test of axial insulation break was performed, further helium tight test and high voltage tests indicate the baked insulation break is in good condition.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.