Abstract
Al–Si–Mg alloys with 7% and 12% (mass ratio) Si contents were subjected to friction stir processing (FSP), warm rolling (WR), and heat treatment. The effects of process routes on the microstructure and mechanical properties of the Al–Si–Mg alloys were studied. FSP could break the eutectic structure and lead to the uniform distribution of the generated fine Si particles in the two Al–Si–Mg alloys. WR could effectively decrease the porosity of the Al–Si–Mg alloys. T6 could lead to the precipitation of the β'′ phases in these alloys. The structure characteristics, including fine grain and second phases, uniformly distributed Si particles, high density of β'′ phases, and low porosity, resulted in the satisfactory mechanical properties of the Al–Si–Mg alloys after FSP, WR, and T6 treatments.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.