Abstract

In order to fabricate high damping/strength metal matrix composites, hard ceramic particulates Li6.75La3Zr1.75Nb0.25O12 (LLZNO) reinforced Al composites were prepared by accumulative roll bonding (ARB) method with intermittent heat treatments. LLZNO particles did not react with Al and were uniformly dispersed in Al-matrix after 10 ARB cycles. With increasing ARB cycles, the ultimate tensile strength of the LLZNO/Al composites increased and reached 132MPa after 10 ARB cycles, which was 2.5 times that of the pure Al, while the total elongation of LLZNO/Al composites increased from 5% after 1 cycle to 10% after 10 cycles. The maximum damping capacity as high as 0.009 was achieved after 10 ARB cycles in the 10wt% LLZNO/Al composite at 320K and 1Hz, which was 4.5 times that of pure Al. The simultaneous enhancement on damping capacity, tensile strength and ductility of the LLZNO/Al composite around room temperature can be ascribed to the high damping capacity and the dispersion strengthening of the LLZNO phase, as well as the good bonding between the LLZNO particles and Al matrix resulted from the ARB technique.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.