Abstract
In this study, we propose highly stable perovskite quantum dots (PQDs) coated with Al2O3 using atomic layer deposition (ALD) passivation technology. This passivation layer effectively protects the QDs from moisture infiltration and oxidation as well as from high temperatures and any changes in the material characteristics. They exhibit excellent wavelength stability and reliability in terms of current variation tests, long-term light aging tests, and temperature/humidity tests (60°/90%). A white-light system has been fabricated by integrating a micro-LED and red phosphor exhibiting a high data transmission rate of 1 Gbit/s. These results suggest that PeQDs treated with ALD passivation protection offer promising prospects in full-color micro-displays and high-speed visible-light communication (VLC) applications.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.